Samarium Cobalt Ring Features
1. Density - 8.3 g/ cm3 (SmCo5), 8.4 g/ cm3 (Sm2Co17)
2. Manufacturing process - sintering
3. High magnetic performance - up to about 32MGOe.
4.Shape :Ring Sintered SmCo
5.Material : Sm2Co17, SmCo5, YXG24, YXG28, YXG30, SMG24, SMG30, SM 20,SM18, YX18
6.Delivery Time : 15-20 working days for prototype or batch accordingly
Quantity:
  • DunBen

sintered SmCo permanent magnets ring

SmCo permanent magnets ring are composed of Samarium, Cobalt and Iron, these rare earth magnets are extremely strong for their small size, metallic in appearance and sable physical property. Those magnets could be in simple shapes also could be made according to customer's need.

Characteristics:
* Resistance to high temperature(max temp reaches 350 degree centigrade)
* Excellent resistance to corrosion
* Low temperature coefficient


 Magnetic property chart:

Grade (Br)
( KGs)
(Hcb)
( Koe)
(Hcj)(Koe) (BH)max
(MGoe)
Tw
SmCo5
YX-5 4.30-5.00 ≥3.80 ≥15 4.0-5.0 ≤250
YX-6 5.00-6.00 ≥4.50 ≥15 5.0-7.0 ≤300
YX-16 7.50-8.50 ≥7.00 ≥15 14-17 ≤250
YX-18 8.50-9.20 ≥8.00 ≥18 16-19 ≤250
YX-20 8.80-9.50 ≥8.30 ≥18 18-21 ≤250
YX-22 9.00-9.80 ≥8.50 ≥15 21-23 ≤250
YX-24 9.5-10.30 ≥9.00 ≥15 22-25 ≤250
Sm2Co17
YX-24A 9.5-10.30 5.0-6.0 6.00-8.50 22-25 ≤200
YX-24B 9.5-10.30 ≥9.00 ≥15 22-25 ≤250
YX-24C 9.5-10.30 ≥9.00 ≥25 22-25 ≤300
YX-24D 9.5-10.30 ≥9.00 ≥30 22-25 ≤350
YX-26A 10.0-10.7 5.0-6.0 6.00-8.50 24-27 ≤200
YX-26B 10.0-10.7 ≥9.00 ≥15 24-27 ≤250
YX-26C 10.0-10.7 ≥9.00 ≥25 24-27 ≤300
YX-26D 10.0-10.7 ≥9.00 ≥30 24-27 ≤350
YX-28A 10.3-11.0 5.0-6.0 6.00-8.50 26-29 ≤200
YX-28B 10.3-11.0 ≥9.00 ≥15 26-29 ≤250
YX-28C 10.3-11.0 ≥9.00 ≥25 26-29 ≤300
YX-28D 10.3-11.0 ≥9.00 ≥30 26-29 ≤350
YX-30A 10.8-11.3 5.0-6.0 6.00-8.50 28-31 ≤200
YX-30B 10.8-11.3 ≥9.00 ≥15 28-31 ≤250
YX-30C 10.8-11.3 ≥9.00 ≥25 28-31 ≤300
YX-30D 10.8-11.3 ≥9.00 ≥30 28-31 ≤350
ZYX-5 4.30-5.00 ≥3.80 8.0-12.0 4.0-5.0 ≤180
ZYX-8 5.00-6.50 ≥4.50 8.0-12.0 6.0-9.0 ≤180
ZSYX ≤6.50 ≤6.0 8.0-12.0 ≤9.0 ≤180
 

Physical Properties of SmCo Magnet

Physical Properties of SmCo Magnet

Material

Sm1Co5

Sm2Co17

Curie Temperature (℃)

700-750

800-850

Max. Operating Temperature (℃)

250

350

Hardness (Hv)

450-500

500-600

Density (g/cm³)

8.2-8.4

8.3-8.5

Temperature Coefficient of Br (%/℃)

-0.05

-0.03

 

Application:

Motors, watch, transducers, instruments, positional detector, generators, radar communications, medical equipments, various magnetism spreading devices, magnetic processor, electrical engineering and magnetic derrick, etc

SMCO applicatons1smco process flow


Previous: 
Next: 

CONTACT US

  Hang Zhou XiaoShan Dunben Magnet  Co., Ltd 
 1702, Unit 2, Building 1, Dacheng Mingzuo, Shiixn Road, Xiaoshan, Hangzhou, Zhejiang, China
  86-571-82750965 
  86-571-82751287
 wang@dbmagnet.com
 

COMPANY

FEEDBACK

Scan QR Code

Copyright © Hang Zhou XiaoShan Dunben Magnet  Co., Ltd All rights reserved.
Designed by Leadong    Manage Entrance